Researchers in China have investigated why screen printing can degrade copper-plated silicon heterojunction (HJT) solar cells and have proposed a modified screen design to reduce the damage. The work focuses on the photoresist-printing step used before copper plating, where the screen comes into broad direct contact with the wafer.
Corresponding author Lang Zhou said the process for applying photoresist differs from conventional silver-paste printing. Silver-paste screens have openings covering only 2–5% of the area, while an emulsion layer protects the rest of the wafer from mesh contact. Full-area photoresist coating typically uses a screen without emulsion to ensure uniform resist deposition, so the mesh touches the wafer directly and extensively in every printing cycle.
Production data cited by the researchers showed conversion efficiency falling from 26.2% to 25.7% over 15,000 consecutive printing cycles. Open-circuit voltage and fill factor accounted for most of the loss, while short-circuit current density and electrical resistance stayed largely unchanged. Minority-carrier lifetime degradation rose from 0.61% with a new screen to 11.0% after 15,000 cycles.
Using three-dimensional confocal microscopy, the researchers linked the decline to progressive wear of the screen mesh knuckles. As these knuckles flattened, their contact area with the wafer increased, raising mechanical stress on the passivation layers. Scanning electron microscopy showed no visible surface scratches, but photoluminescence measurements indicated higher recombination losses, pointing to damage near the amorphous silicon/crystalline silicon interface.
Buffer layer balances protection and coating
To reduce contact, the team added an emulsion buffer layer to the screen and tested six patterns with emulsion coverage from 2.9% to 16.6%. Higher coverage protected the wafer better but impaired ink distribution, creating a trade-off between mechanical protection and coating uniformity.
A 4.7% emulsion coverage ratio gave the best balance in the reported experiments. After 10,000 printing cycles, minority-carrier lifetime degradation was limited to 0.41%, while coating uniformity remained relatively good. The researchers attributed the improvement to the emulsion layer preventing direct contact between the mesh and the wafer, reducing cumulative mechanical damage to the sensitive passivation layers.
Zhou said the results demonstrate that a relatively simple modification to screen design can substantially mitigate printing-induced degradation, offering a practical approach to improving manufacturing reliability for copper-plated HJT cells. The findings were published in Solar Energy.
Copper metallization gains attention
The screen-design work comes as HJT developers examine copper plating to reduce silver consumption and metallization costs. Copper contacts can replace silver, but the processes must protect the sensitive passivation stack and maintain adhesion and contact quality.
In April 2026, researchers at China's Nankai University reported a silver-free HJT solar cell with 25.2% efficiency. The approach combined plasma-induced interface engineering with copper electroplating and addressed adhesion, contact resistance and stability challenges at the indium tin oxide interface.
Separately, scientists at Germany's Forschungszentrum Jülich achieved 23.08% efficiency in a fully copper-metallized HJT cell. The silver-free device showed a relatively small efficiency penalty compared with its silver-metallized counterpart, while a cell combining silver-copper paste on the front side with silver contacts on the rear reached 23.95% efficiency. Those results underline copper's potential to reduce silver use, although further improvements in processing and electrical performance remain necessary.